Story | Introduction | Advantage | Testing | Application
Since COPPRON is a new kind of fiber, it is only determined as "other fiber" by any testing agency who has never studied on COPPRON.
So far, The State Wool Textile Products Quality Supervision & Test Center (The Woolmark Company Authorized Test Center- TWC) has rich experience in qualitative and quantitative detection of COPPRON. And also the detection could be outsourced to TWC from SGS with test report.
Internationally, COPPRON can be labeled by "copper modify acrylic fiber" or "copper & other fiber".
COPPRON Fiber |
Testing Standard: FZ/T 73023-2006 |
Test Sample |
Bacteria |
Bacteria Amount at “0” Hour |
Bacteria Amount after Germiculture |
Reduction |
COPPRON Fiber |
|
/ |
1.0*10^2 |
>99.9% |
Control Group |
Staphylococcus Aureus |
9.2*10^3 |
4.8*10^6 |
/ |
COPPRON Fiber |
|
/ |
2.1*10^5 |
99.6% |
Control Group |
Colibacillus |
2.5*10^4 |
5.8*10^7 |
/ |
COPPRON Fiber |
|
/ |
9.9*10^3 |
98.8% |
Control Group |
Candida Albicans |
8.5*10^3 |
8.2*10^5 |
/ |
COPPRON Yarn(5% COPPRON Fiber 95% Cotton) |
Testing Standard: GBT 20944.3-2008 |
Test Sample |
Bacteria |
Bacteria Amount at “0” Hour |
Bacteria Amount after Germiculture |
Reduction |
COPPRON Yarn |
|
/ |
1.3*10^3 |
>99% |
Control Group |
Staphylococcus Aureus |
1.2*10^4 |
1.2*10^7 |
/ |
COPPRON Yarn |
|
/ |
1.7*10^7 |
87% |
Control Group |
Colibacillus |
2.5*10^4 |
1.3*10^8 |
/ |
COPPRON Yarn |
|
/ |
8.8*10^4 |
97% |
Control Group |
Candida Albicans |
1.1*10^4 |
2.6*10^6 |
/ |
anti-microbial self-clean fabric
fabric comp-osition:5%COPPRON ions fiber,
70%cotton+25%core-spun yarn of spandex in polyamide
|
Test Items |
Test Standards |
Test Results |
Unit |
Dcodorant rate |
Ammonia |
Refer to part 21 of SEK standard provided by Japan textile evaluation technology council |
98 |
% |
Acetic acid |
96 |
Isovaleria acid |
95 |